Spatters

DEFECT WELD
(VISUAL)

SPATTERS


Defect Weld : Spatters


Because :
1. Environmental wet or moist.
2. Elektoda moist.
3. The wind getting into the area welds.
4. The arc welding too long .
5. Capping current too high.
6. Kind of a current wrong.
7. Kinds of polarity wrong.
8. The galvaniize not yet been grinding.

Result :
1. Bad Profile
2. Started rust the surface
               
Countermeasures :
1 . Use chisel only or niggardly churlish .Do not use grindstone because it is going to take the base metal

Rejection criteria : If not cleared can cause rejection (Because it is not relevant with standard)