POROSITY

DEFECT WELD 
(VISUAL)

POROSITY

Defect Weld : Porosity


Because :
1. Environmental wet or moist.
2. The galvaniize not yet been grinding .
3. Elektoda moist.
4. A rising gas when welding prosses.
5. Ampere capping too high .
6. The wind getting into the area welds.
7. Welding-joint dirty.

Result
1. Bad Profile.
2. Weaken weld joint.
3. Started rust the surface.

Countermeasures :
Grinding or gouging to defect missing, Welds repeated according WPS repair

Rejection criteria :
1. Individually to exceed 1/8” or 25% nominal thickness.
2. For cluster porosity Diameter more than ½”.

3. The number of long clusters in 12” weld more than ½”.