BLOW HOLE

DEFECT WELD
NON VISUAL


BLOW HOLE

Blow Hole


Because :
1. ELEKTRODA UP DOWN
2. GAP NO CONSISTENT
3. AMPERE ROOT SWING

Result :
Started erosion abrasion.

Countermeasures :
1. Gouging until roots in the location of a defect in the welds and appropriate contents WPS REPAIR.

Rejected Criteria
API 1104 : For the use of normal or SEVERE CYCLIC must repair, if not , it’s reject. In the d is still could be accepted as long as :
1. INDIVIDUAL ≤ 1/4 “ or thick plate .
2. If the number of long in 12” lasan < ½ “.